Investigation into Flotation Properties of New Collectors
when Concentrating Scheelite–Sulfide Ores
L. A. Samatovaa, *, V. I. Ryaboyb, **, and E. D. Shepetaa, ***
Translated by N. Korovin
a Institute of Mining, Far East Branch, Russian Academy of Sciences, Khabarovsk, 680000 Russia
b OOO Mekhanobr-Orgsintez-Reagent, St. Petersburg, 199155 Russia
Correspondence to: *e-mail: samatova_luiza@mail.ru
Correspondence to: **e-mail: frim@isc1.nw.ru
Correspondence to: ***e-mail: elenashepeta56@mail.ru
Received 31 May, 2016
Abstract—Flotation properties of dialkyl dithiophosphates of alkali metals BTF-1552, IMA-206, and IMA-I413 are investigated. Concentration characteristics using the M-TF reactant and its mixture with IMA-I413 and xanthate are evaluated. Based on these investigations, it is established that the application of the mixture of collectors IMA-I413 and butyl xanthate in the ratio 5 : 1 with the consumption of 20 + 5 g/t makes it possible to increase the recovery into the copper concentrate by 0.79% for Cu, by 4.1% for Au, and by 2.4% for Ag with a twofold decrease in the yield of the sulfide concentrate. The disadvantage of this composition of reactants is an increase in the As content in the copper concentrate by 0.67%. The better characteristics by an increment of recovery of copper and precious metals among the tested samples are observed for the BTF-1552 collector. The recovery into the copper concentrate increased by 1.9% for Cu, by 3.2% for Au, and by 1.8% for Ag with a decrease in the yield of the sulfide concentrate by a factor of 1.4. An increase in the As content in the copper concentrate is 0.34%.
Keywords: skarn ores, scheelite, sulfide minerals, flotation, selective collectors, aeroflot agents, xanthates