Crazing of Isotactic Polypropylene
in the Medium of Supercritical Carbon Dioxide1
E. S. Trofimchuka, A. V. Efimova, N. I. Nikonorovaa, A. L. Volynskiia,
N. F. Bakeeva, L. N. Nikitinb, A. R. Khokhlovb, and L. A. Ozerinac
a Faculty of Chemistry, Moscow State University, Moscow, 119991 Russia
b Nesmeyanov Institute of Organoelement Compounds, Russian Academy of Sciences, ul. Vavilova 28, Moscow, 119991 Russia
c Karpov Institute of Physical Chemistry, ul. Vorontsovo pole 10, Moscow, 105064 Russia
e-mail: elena_trofimchuk@mail.ru
Received September 30, 2010;
Revised Manuscript Received January 11, 2011
AbstractUniaxial tensile drawing of films based on semicrystalline isotactic PP in the medium of supercrit-
ical carbon dioxide at a pressure of 10 MPa and a temperature of 35C is studied. The tensile drawing of PP is
shown to proceed in the homogeneous mode without necking and is accompanied by intense cavitation. The
maximum level of porosity is 60 vol %. The porous structure that develops owing to the tensile drawing of the
polymer in supercritical CO2 is provided by formation of a set of crazes that are primarily localized in inter-
lamellar regions. According to small-angle X-ray scattering data, the average diameter of fibrils that bridge
craze walls changes slightly with an increase in tensile strain and is ~10 nm; the specific surface of the craze
fibrils is 100150 m2/cm3.
DOI: 10.1134/S0965545X11050154